Rayresin

Bicomponent epoxy resin for installations up to 1 kV

Resin for electrical insulation and for the protection of thermosetting LV and MV accessories. The two components, the base resin and hardener, are mixed in close contact to trigger the cross linking reaction. Excellent bonding to metal, plastic and rubber components.

Cross linking time:
20 minutes at 20°C
Hardness:
70 Shore D
Dielectric strength:
21 kV/mm
Specific weight:
1,07 kg/dm³
1,7 kg/dm³ for Rayresin Tan 3,8
Water absorption:
0,8% max

RAYRESIN 170

RAYRESIN 210

RAYRESIN 420

RAYRESIN TAN 3.8